Flame retardant description:

1. Mainly contents with nitrogen, phosphorus, and bromine.

2 .Easy to use, no need to add antimony trioxide etc.

3. With 1-2% dosage in Homopolymerization pp. 3-4% dosage in Copolymerization PP flame retardant, available for flame retardant granule manufacture in mixing of Copolymerization and Homopolymerization PP together.

Features:

Lower dosage

self-extinguishing from fire

High-cost effective

Non-blooming

good thermal stability

 good water resistance

light aging resistance

good mechanical properties

 

Application:

PP foam flame retardant, polypropylene foam flame retardant, automobile foam flame retardant

 

Flame property

UL94-V2

Remarks:

1.During using, no need to add antioxidant, antimony oxide or other additional agent.

2. Also can be used in modified granulation of Homopolymerization pp and Copolymerization PP.

3. Barium sulfate or talcum powder (talcum powder cannot contain calcium carbonate) can be filled with flame retardants, dosage at 15-20%.

4. In order to increase dispersity and lubricity, white oil and EBS can b added appropriately.

Performance:

Appearance

White   powder

The Content of Bromine

 12%

 The Content of Phosphorus

8 %

The Content of Nitrogen

 5%

weightless   temperature ℃

≦0.5%

TGA(5%)

275℃ 

Dosage

1-2%


Flame Retardancy Standard